Products Of Combustion
Hi Yogesh,
Good question. Problem solving is like detective work. You have to get the clues, then propose a theory, then go back and look for more clues to either back up or reject the theory.
Some questions to ask
1 - What is the chemical analysis of the snowman formation? There are many products of combustion in a kiln.
2 - Do any of the raw materials affect it? Good question. How can you verify it?
3 - Are you introducing flux? Where and how?
4 - Is there a temperature gradient at the Cooler entry? Does this have any significant effect.
5 - Look at the variables, and what are the consequences of
-- High flow, Low flow
-- High temperature, Low temperature
-- High flux, Low flux
Best of luck - John.rz ■
Untitled
Dear Sir,
Thank you very much for your valuable suggetions ■
Snow man formation in clinker cooler
Dear sir,
In our plant we are facing frequent snowman formation problem (formation of heeped coatings near cooler inlet and kiln hood).We are using 6 blasters of 5 kg/cm2 pressure which are operating normally. May I know what are the reasons for the formation of this type of coatings(snowman)? Does any of the raw material properties effects the coating formation
Regards,