Antworten
Re: Material Spec
Erstellt am
2. Jan. 2008 - 10:49
According to my books 42CrMo4 approximates chemically to 709M40 (the old EN19).
709M40 can be treated up to condition V (1000/1160 N/mm2) on a 29mm ruling section.
42CrMo4 can be treated to 980/1080 n/mm2 on a 40mm ruling section.
Hope this helps. ■
Material Spec